Table 22.

X ray micro densitometric components of specimens attacked by fungi [59].

Wood species Specimens
X ray micro density components (kg/m3)
Earlywood Average Latewood D min D Max
White rot – Lignin attack
Beech Control 660 697 789 591 853
Five months 490 524 583 439 638
Difference % 25.7 24.8 26.1 25.7 25.2

Brown rot – Cellulose attack
Pine Control 455 602 920 377 1012
Five months 360 420 546 324 607
Difference % 20.8 30.2 40.6 16.3 40.0